2 Best Things About Friction And Lubrication in the Stamping Process

صورة مميزة

الوقت المقدر للقراءة: 9 دقيقة

الاحتكاك على عملية الختم

ال عملية الختم is very important, the sheet is always in contact with the die. This contact is not static, but dynamic. Because the metal sheet flows over the die surface, there is relative motion between the sheet and the die. Even though sheet and mold surfaces appear smooth without visual aid, under the microscope, their surfaces show complex shapes. Stamping Process

عملية الختم
الشكل 1: صفائح الفولاذ الطري غير المطلية بخشونة 1.5 ميكرومتر
الشكل 2 سطح أداة الحديد الزهر مع خشونة 0.4 ميكرومتر
الشكل 2: سطح أداة من الحديد الزهر مع خشونة 0.4 ميكرومتر

Sheet and tool surfaces have roughness distributions that consist of a series of peaks and valleys of varying heights, depths, and spacings, as shown in Figures 1 and 2. The roughness distribution of sheet metal will vary depending on the type, grade, and coating of the material, while the roughness distribution of tools will vary depending on the type of material and how they are processed. Stamping Process

Due to these irregularities of the sheet and tool surfaces, there is resistance to relative motion. In simple terms, this resistance to relative motion is called “friction”, which is why lubricants are applied to metal plates to reduce their resistance and therefore friction. The ratio between the frictional force and the contact force of two moving objects is represented by the coefficient of friction “μ”, the value of which depends on the tribological system itself and the forming process, such as the temperature of the sheet, the stamping speed, the contact pressure and the strain of the sheet. Stamping Process

تزييت على ختم بروسيس

We know where the friction is coming from and why we need to lubricate the sheet before stamping. We will now focus on how the amount of lubrication affects the quality of the panels during the forming process. You can get a better understanding of the lubrication effect through the pictures below. Stamping Process

الشكل 3 كمية التشحيم عالية جدًا
الشكل 3: كمية التشحيم عالية جدًا في الختم
الشكل 4 كمية التشحيم منخفضة للغاية
الشكل 4: كمية التزييت منخفضة للغاية
الشكل 5 التزييت الأمثل
الشكل 5: التشحيم الأمثل

تمت محاكاة الأوراق الموضحة في الأشكال 3 و 4 و 5 باستخدام نفس إعداد المحاكاة الدقيق ، وكانت جودة الجزء مختلفة لأن كمية مادة التشحيم قد تغيرت. اللوح الموضح في الشكل 3 به تجعد شديد في الزوايا بسبب التشحيم العالي المطبق على الصفيحة قبل التمدد.

The higher the amount of lubrication, the lower the resistance to movement, i.e. the material then moves freely over the tool surface in an uncontrolled manner, creating wrinkles. Conversely, when the amount of lubrication applied to the sheet is very low, the resistance to motion is very high. This high resistance forces the sheet metal to stretch beyond the desired amount, producing substantial thinning and, in some cases, extensive cracking, as shown in Figure 4. Stamping Process

Therefore, it becomes critical to use the proper amount of lubrication when pulling panels, as is finding the optimum amount of lubrication required. Figure 5 shows a sheet without wrinkles and cracks when the lubricant is properly applied. Stamping Process

تمامًا مثل أي عملية تصنيع أخرى ، يؤدي تطبيق مادة التشحيم على الصفيحة إلى بعض التناقضات مثل الضوضاء. هذا يعني ، إذا قرر المستخدم استخدام 1 جم / م 2 من مادة التشحيم على الصفيحة ، وبالتالي إنتاج لوحة خالية من العيوب ، فما هو احتمال أن يقوم الروبوت برش الكمية الدقيقة من مادة التشحيم على اللوحة في كل مرة؟ على سبيل المثال ، إذا كانت دقة الجهاز 85% ، فإن انحراف مادة التشحيم سيكون 0.85 - 1.15 جم / ، إذا كانت اللوحة حساسة جدًا للاحتكاك ، فقد تكون هناك بعض المشكلات. لذلك ، من الأهمية بمكان العثور على مجموعة آمنة من كميات التزييت والتأكد من أن الجهاز يقوم برش مادة التشحيم ضمن النطاق المحدد.

When considering an AHSS stamping tribology system, there are three main points to consider, namely: 1. The effect of friction and tribology on spring back; 2. AHSS stamping produces higher temperatures, which again affects friction behavior; 3. The use of different tool materials in AHSS stamping has new effects on the friction behavior informing and simulation. These three phenomena should be considered in stamping simulations, which can only be achieved by using advanced stamping friction models. Stamping Process

الشكل 6 آلة التثقيب HARSLE JH21
الشكل 6: آلة تثقيب HARSLE JH21

بالطبع ، يتمتع AHSS بمزيد من الربيع عند ختم الأجزاء الحساسة. يمكن أن يتأثر الارتداد الخلفي بشدة بسلوك الاحتكاك المحدد في الصفائح المعدنية تشكيل simulation. This is why you should improve the friction behavior in punch simulations. This, in turn, yields better rebound predictions. Friction determines the amount of restraint in the part, and based on this, spring-back behavior is affected. Stamping Process

Also, it is important to consider that during AHSS stamping, higher contact pressures between the tool and the sheet are often observed, which is why friction becomes so important, and friction causes an increase in temperature in the material, which For mild steel, this order of magnitude does not occur. Therefore, a proper description of temperature variation and its effect on frictional behavior is critical for simulating the stamping of AHSS. Stamping Process

Additionally, AHSS stamping materials require the use of tool steels that are not typically used on medium strength steels. Now we have to consider the tribological effects of harder tools made of a certain carbon and chromium content, rather than tools made of cast iron. This mold material also has an effect on tribological properties. This is why the user must take this into account as well as lubricant selection during the simulation setup. A good friction model should take into account all these interrelationships when generating the friction model. Stamping Process

If you have an advanced friction model in your forming simulation, then you need to introduce a realistic tribology system in your sheet metal forming simulation. You’ll then get more accurate crack, wrinkle, thinning, and spring back predictions, all tied to the friction model you’re using. Stamping Process

In the process of deep drawing, due to the relative movement between the workpiece and the surface of the mold, adhesion will occur under the action of a certain pressure. When stainless steel is deep-drawn, this phenomenon is more serious, resulting in scratches on the surface of the product and the appearance of the mold surface. “Bonding nodules”, in order to protect the surface quality of products, control friction, wear, and remove scratches, the most effective means is lubrication. The first point of selecting lubricant is that the lubricating film does not break and lubricates throughout the sheet metal deep drawing process. Stamping Process

“Anti-viscosity and friction reduction” is the basic starting point for selecting lubricants. Under the premise that other conditions meet the deep drawing process, the quality of lubrication will directly affect the drawing force, die life and product quality, etc., and even become the key to the success or failure of the deep drawing process. According to the information, among various processes, the deep drawing process consumes the most amount of lubricant. During the deep drawing process, due to the relatively large deformation of the material, the lubricant is required to have excellent performance. Stamping Process

دعونا نلقي نظرة على مواد التشحيم المختلفة:

الشكل 7 مواد تشحيم ختم مختلفة
الشكل 7: زيوت التشحيم المختلفة

فيما يلي خصائص العديد من مواد التشحيم الشائعة:

اكتبمزاياعيب
زيوت معدنية1. معترف بها على نطاق واسع وتستخدم في الصناعة
2. الكلور والكبريت من المضافات التزييت الفعالة للغاية عند الضغط الشديد
3. عادة ما تحافظ على رطوبة قطعة العمل ، ولا يكون التصاق قطعة العمل خطيرًا أثناء الاستخدام
1. تكنولوجيا عفا عليها الزمن ، تقدم ضئيل في البحث والتطوير
2. صعب الخلط ، مستحلب غير مستقر
3. يحتوي على مكونات ضارة وقابلة للاشتعال
4. من الصعب تنظيف اللحام وتوجيهه
5. زيادة رسوم المعالجة
زيت متطاير1. يمكن أن تتبخر من قطعة العمل
2. سهلة التنظيف
1. سامة وقابلة للاشتعال
2. يسبب أمراض جلدية خطيرة
3. حماية أقل للأدوات
4. لا تختفي تماما
5. يتجاوز الحد الأقصى لكمية المركبات العضوية المتطايرة في الهواء
6. زيادة محتوى المركبات العضوية المتطايرة بشكل كبير في ورشة العمل
الفيلم الجاف والصابون المحفور1. يخلط مع زيت التشحيم أو يستخدم بمفرده أثناء الختم
2. منتجات تزييت فعالة للغاية
1. بناء على القالب
2. تولد جزيئات البورق في الثقب
3. أضف تكلفة إضافية عند تنظيف القالب
4. الرغوة عند التنظيف
5. سوف تصبح لينة ولزجة في بيئة رطبة أو عند مواجهة مواد التشحيم
6. أخطأ كمعدن ثقيل في مياه الصرف الصحي
مركب صابون1. منتج حماية أداة عالمية
2. السعر المنخفض
3. لا تزال فعالة بعد التخفيف
1. تكنولوجيا ثلاثينيات القرن التاسع عشر
2. لا تحتوي على إضافات EP
3. الصباغ متصل بالأداة ، وجزء الختم عرضة للالتصاق
4. لزوجة السطح لقطع العمل كبيرة
5. تآكل المعادن اللينة
6. الرغوة أثناء التنظيف
خصائص العديد من مواد التشحيم الشائعة

During the lubrication process, different vaporization will occur as the temperature rises, taking away a lot of heat, thereby reducing the temperature of the mold; as the vaporization continues to generate, the lubricant will continue to accumulate to the high-temperature point, forming a tougher The lubricating film protects the mold more effectively, thereby extending the service life of the mold. It will also improve the quality of the workpiece surface without scratches, as shown in the figure below. Stamping Process

الشكل 8 تحسين جودة السطح للأجزاء المختومة
الشكل 8: تحسين جودة السطح للأجزاء المختومة

اللكم ماخine للبيع

أفكار 2 على "2 Best Things About Friction And Lubrication in the Stamping Process"

  1. يقول Tony Jothson:

    المقال ممتع جدا! هل لديك JH21-160T في المخزون؟ هل يمكنك إخباري بالسعر؟

    1. يقول Wendy:

      نعم لدينا!
      من فضلك قل لي صندوق البريد الخاص بك ، وأرسل لك عرض أسعار.

اترك تعليقاً

لن يتم نشر عنوان بريدك الإلكتروني. الحقول الإلزامية مشار إليها بـ *